气凝胶内墙保温涂料(净味型)HUALU Pyshield AC-JZ-01N01
南方潮湿所引起的发霉、结露以及冬日体感的湿冷现象,核心原因都在于室内的湿度及房屋的隔热节能效果差。使用气凝胶内墙涂料以后,能够隔绝
墙内水分,提升室内结露点。减少房间湿冷感。提高空调使用效率,降低能耗。
产品优势
1.极致节能,省电省费(温度最高可降低10℃,空调节电率最高可达30%)
2.以1-2毫米的极致厚度,美传统材料数厘米厚的效果
3.持久疏水,防潮防霉
4.安全环保,净味除醛
5.施工便捷,适用性广
6.可提供多重艺术效果
产品参数
|
项目 ltem |
参数 Parameter |
|||
|
颜色 Color |
白(可调) White(customizable) |
|||
|
导热系数 Thermal Conductivity |
0.04W/(m·k)@25℃℃ | |||
|
密度 Density |
0.54±0.03 g/cm³ | |||
|
粘结强度 Bond Strength |
≥0.6 MPa | |||
|
耐水性 Water Resistance |
浸水96h无异常 No abnormality after 96h immersion |
|||
|
燃烧性能 Combustion Performance |
B2 | |||
|
VOC含量 VOC Content |
≤50 q/L | |||
|
柔韧性 Flexibility |
直径100 mm无裂纹 No cracks at 100 mm diameter |
|||
|
初期干燥抗裂性(6h) Initial Drying Crack Resistance(6h) |
2 mm无裂纹 No cracks at 2 mm |
|||
|
规格 Specification |
10 kg/20 L | |||
|
用量 Usage |
0.6(kg/mm/㎡) | |||
图层设计结构
|
项目 ltem |
参考厚度(mm) Reference Thickness(mm |
|||
| 内墙耐水腻子 Interior Waterproof Putty |
3-5 mm | |||
|
抗碱封闭底涂 |
<0.5 mm | |||
| 气凝胶内墙保温涂料(净味型) Interior Aerogel Thermal insulation Coating (Low-Odor Type) |
2-3 mm | |||
|
饰面层 Finish Layer |
<0.3 mm(可定制) | |||

产品应用
气凝胶内墙保温涂料(净味型)可用于家庭装修、商业空间、公共空间等。气凝胶涂料隔汽防潮、隔热保温、轻量化特质与优异隔音性能,有效避免因温湿度差导致的墙体结露问题,进而彻底杜绝霉菌滋生,长久保持墙面干爽洁净,为建筑环境筑牢健康防线,提升居住舒适度与墙体使用寿命、降低能耗。

施工要求
|
项目 ltem |
喷涂 Spray Coating |
|||
| 基面要求 Surface Requirements |
涂层施工前,先将墙体表面的油污、灰尘、空鼓、开裂、脱落等异常情况,采用找平腻子填补(挂网),基面平整、干燥,要求墙体含水率小于10%,pH值小于9。 Application, remove oil stains, dust, hollow areas, cracks, peeling, and other abnormalities from the wall surface. Level with putty(with mesh reinforcement if necessary). The surface must be flat, dry, with a moisture content below 10% and ph below 9. |
|||
|
施工工具 |
喷涂机、辊筒、美纹纸、搅拌器、防护口罩、防护服、安全绳、安全帽、防护鞋、护目镜、保护膜 Spray machine, roller, masking tape, mixer, protective mask, protective clothing, safety rope, safety helmet, safety shoes, goggles protective film |
|||
| 施工工艺 Mixing Instructions |
开桶搅拌:请先检查涂层原料有无明显分层现象,如有分层现象可用搅拌方式搅拌均匀,不可高速分散。搅拌时间应在3-5分钟,喷涂施工厚度单次不超过2 mm,间隔12小时后再重喷,具体厚度可商定。 Open the container and stir: First check for significant stratification in the coating material, f stratification is observed, mix uniforml by stirring-do not use high-speed dispersion, Stir for 3-5 minutes, The construction thickness should not exceed 2mm per application, and re-spraying should be performed after an interval of 12 hours. The specific thickness can be customized. |
|||
| 施工条件 Construction Conditions |
1.施工温度不低于5℃。 2.避免刮风下雨天气施工。 |
|||