图片编辑-5

气凝胶隔音涂料 HUALU Pyshield AC-JZ-02GY01

气凝胶隔音涂料采用超高孔隙率纳米气凝胶和高分子弹性材料复合而成,常温固化,涂层致密,能有效阻碍声波传递,减少透射声能,降低分贝,同时兼具一定的保温效果,适用于建筑楼板等隔音减振。

产品优势

1.毫米级(1-3 mm)涂覆,超越传统厘米级隔音效果
2.优异的阻燃性能
3.降低分贝量>15分贝
4.防潮防腐,性能稳定
5.施工便捷,适应性强

 

产品参数

 

项目

ltem

参数

Parameter

吸水量

Water Absorption, %

≤15

初期抗开裂

Initial Crack Resistance

3h无裂纹

No cracks after 3h

粘接强度

Mpa Bond Strength, MPa

>0.2
柔韧性 Flexibility

直径50 mm无裂纹

No cracks at 50 mm diameter

干燥时间(实干),天

Drying Time(Cured),days

≤3
低温稳定性,3个循环
Low-Temperature Stability, 3 cycles

不变质

No deterioration

甲醛含量,mg/kg

Formaldehyde Content, mg/kg

≤15
挥发 Usage合物(VOC),g/L
Volatile Organic Compounds (VoC), g/L
≤50
5 mm 厚涂膜,撞击声改善量
lmpact Sound lmprovement (5 mm thick coating)
≥15 dB

规格

Specification

10 kg/20 L

用量

Usage

0.6(kg/mm/㎡)

 

 

图层设计结构

 

项目

ltem

参考厚度(mm)
Reference Thickness(mm
瓷砖
Tile
10 mm

普通水泥砂浆
Ordinary cement mortar

40 mm
气凝胶隔音涂料
Aerogel Soundproofing Coating
3-5 mm
钢筋混凝土楼板
Reinforced concrete slab
140 mm

 

 

 

 

 

产品应用

适用于住宅、办公楼、学校、医院、酒店宾馆、图书馆等有隔音要求的场所或空间,建筑楼板的隔音减振,提高楼板、地面的减震效果,达到隔声的目的。

 

 

 

施工要求

 

项目

ltem

喷涂

Spray Coating

基面要求
Surface Requirements
涂层施工前,先将墙体表面的油污、灰尘、空鼓、开裂、脱落等异常情况,采用找平腻子填补(挂网),基面平整、干燥,要求墙体含水率小于10%,pH值小于9。
Application, remove oil stains, dust, hollow areas, cracks, peeling, and other abnormalities from the wall surface. Level with putty(with mesh reinforcement if necessary). The surface must be flat, dry, with a moisture content below 10% and ph below 9.

施工工具
Tools Required

喷涂机、辊筒、美纹纸、搅拌器、防护口罩、防护服、安全绳、安全帽、防护鞋、护目镜、保护膜
Spray machine, roller, masking tape, mixer, protective mask, protective clothing, safety rope, safety helmet, safety shoes, goggles protective film
施工工艺
Mixing Instructions
开桶搅拌:请先检查涂层原料有无明显分层现象,如有分层现象可用搅拌方式搅拌均匀,不可高速分散。搅拌时间应在3-5分钟,喷涂施工厚度单次不超过2 mm,间隔12小时后再重喷,具体厚度可商定。
Open the container and stir: First check for significant stratification in the coating material, f stratification is observed, mix uniforml by stirring-do not use high-speed dispersion, Stir for 3-5 minutes, The construction thickness should not exceed 2mm per application, and re-spraying should be performed after an interval of 12 hours. The specific thickness can be customized.
施工条件
Construction Conditions

1.施工温度不低于5℃。

2.避免刮风下雨天气施工。
1.Ambient temperature should not be below 5°C.
2. Avoid construction during windy or rainy weather.

点我购买