气凝胶节能防烫涂料 HUALU Pyshield AC-GY-01H200
产品优势
1.卓越的施工适应性
2.完美契合预制化与模块化施工
3.根除保温层下腐蚀
4.优异的耐久性与美观性
5.广泛的基材适用性
6.显著的综合性价比(可减少热损失20%以上)
7.精准解决 “最后一公里”热桥难题
产品参数
|
项目 ltem |
参数 Parameter |
|||
|
颜色 Color |
白(可调) White(customizable) |
|||
|
导热系数 Thermal Conductivity |
≤0.035W/(m·k)@25℃℃ | |||
|
密度 Density |
0.54±0.03 g/cm³ | |||
|
粘结强度 Bond Strength |
≥0.6 MPa | |||
|
耐水性 Water Resistance |
浸水96h无异常 No abnormality after 96h immersion |
|||
|
燃烧性能 Combustion Performance |
B1 | |||
|
VOC含量 VOC Content |
合格 Qualified |
|||
|
柔韧性 Flexibility |
直径50 mm无裂纹 No cracks at 50 mm diameter |
|||
|
初期干燥抗裂性(6h )Initial Drying Crack Resistance(6h) |
<150℃ | |||
|
规格 Specification |
10 kg/20 L | |||
|
用量 Usage |
0.6(kg/mm/㎡) | |||
图层设计结构
|
项目 ltem |
参考厚度(mm) Reference Thickness(mm |
|||
| 底涂 Primer |
30-50μm | |||
|
气凝胶节能防烫涂料 |
2-6 mm | |||
| 面漆 Top Coat |
20-30 μm | |||

产品应用
气凝胶节能防烫涂料广泛应用于石油天然气、化工、电力、船舶海工、冶金、食品饮料等工业领域。可有效减少工业设备、管道和储罐等的热损失,从而提高能源效率,降低运营成本。

施工要求
|
项目 ltem |
喷涂 Spray Coating |
|||
| 基面要求 Surface Requirements |
涂层施工前,先将墙体表面的油污、灰尘、空鼓、开裂、脱落等异常情况,采用找平腻子填补(挂网),基面平整、干燥,要求墙体含水率小于10%,pH值小于9。 Application, remove oil stains, dust, hollow areas, cracks, peeling, and other abnormalities from the wall surface. Level with putty(with mesh reinforcement if necessary). The surface must be flat, dry, with a moisture content below 10% and ph below 9. |
|||
|
施工工具 |
喷涂机、辊筒、美纹纸、搅拌器、防护口罩、防护服、安全绳、安全帽、防护鞋、护目镜、保护膜 Spray machine, roller, masking tape, mixer, protective mask, protective clothing, safety rope, safety helmet, safety shoes, goggles protective film |
|||
| 施工工艺 Mixing Instructions |
开桶搅拌:请先检查涂层原料有无明显分层现象,如有分层现象可用搅拌方式搅拌均匀,不可高速分散。搅拌时间应在3-5分钟,喷涂施工厚度单次不超过2 mm,间隔12小时后再重喷,具体厚度可商定。 Open the container and stir: First check for significant stratification in the coating material, f stratification is observed, mix uniforml by stirring-do not use high-speed dispersion, Stir for 3-5 minutes, The construction thickness should not exceed 2mm per application, and re-spraying should be performed after an interval of 12 hours. The specific thickness can be customized. |
|||
| 施工条件 Construction Conditions |
1.施工温度不低于5℃。 2.避免刮风下雨天气施工。 |
|||